Material Type

Metal

Material Sub-Type

Tool Steel

Material Name

Tool Steel S7

Tool steel S7 is a type of shock-resistant and air-hardening steel. It is commonly used in the manufacturing of tools and dies due to its ability to withstand high impact and retain its hardness at high temperatures. S7 tool steel is also resistant to wear and abrasion, making it well-suited for use in demanding applications. It is often used in the aerospace, automotive, and construction industries.

Cost
Lead Time

4-5 Days

Processes

CNC Machining

Metric

English

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Last Updated:2 months ago
Mechanical Properties

Yield Tensile Strength

1999 MPa

Ultimate Tensile Strength

2151 MPa

Tensile Modulus

207 GPa

Shear Strength

-

Shear Modulus

-

Fatigue Strength

-

Elongation At Break

7 %

Poisson's Ratio

-

Hardness

55 HRC

Density

7.8 g/cm³

Impact Strength (ASTM)

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

-

Magnetism

Moderate

Thermal Properties

Heat Deflection Temperature

190 °C

Thermal Expansion Coefficient

11.0 µm/(m⋅°C

Specific Heat Capacity

-

Thermal Conductivity

44 W/(m⋅°C)

Melting Point

-

Chemical Properties

Corrosion Resistance

Poor

Tool Steel S7

Shock-resistant and easy-to-machine tool steel

Get your parts manufactured today.

Get Instant Quote

Material Datasheet

Material Type

Metal

Material Sub-Type

Tool Steel

Material Name

Tool Steel S7

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Mechanical Properties

Yield Tensile Strength

1999 MPa

290.0 Ksi

Ultimate Tensile Strength

2151 MPa

312.0 Ksi

Tensile Modulus

207 GPa

30.0 Msi

Shear Strength

-

-

Shear Modulus

-

-

Fatigue Strength

-

-

Elongation At Break

7 %

-

Poisson's Ratio

-

-

Hardness

55 HRC

-

Density

7.8 g/cm³

0.283 lb/in³

Impact Strength (ASTM)

-

-

Electrical/Magnetic Properties

Surface Resistance (ANSI)

-

-

Magnetism

Moderate

-

Thermal Properties

Heat Deflection Temperature

190 °C

374 °F

Thermal Expansion Coefficient

11.0 µm/(m⋅°C

6.1 µin/(in⋅°F)

Specific Heat Capacity

-

-

Thermal Conductivity

44 W/(m⋅°C)

25.4 BTU/(h⋅ft⋅°F)

Melting Point

-

-

Chemical Properties

Corrosion Resistance

Poor

-

www.protoxyz.com